logo comp4

Nickel Laterite Sample Preparation Procedure

2 sample preparation the leaching procedure was performed in a 100 ml teflonlined stainless steel autoclave certain amount of hydrochloric acid solution 2 2 and 2 moll 1 was added to the teflon linerhen the limonite laterite ore 10 g, 150 m.